A333 õmblusteta süsinikterasest torud
Tarneaeg: 8-14 päeva
Sektsiooni kuju: ümmargune
Pinnatöötlus: külmvaltsitud
Tolerants: ±1%
Õlitatud või õlitamata: õlitamata
Arveldamine: tegeliku kaalu järgi
A333 õmblusteta süsinikterasest torud
ASTM A333 on õmblusteta ja keevitatud süsinik- ja legeerterasest torude standardspetsifikatsioon krüogeenseks hoolduseks või muudeks rakendusteks, mis nõuavad sälku sitkust. Standard hõlmab mitut ferriitterase klassi: klass, 3. klass, 4. klass, 6. klass, 7. klass, 8. klass, 9. klass, 10. klass ja 11. klass.

|
Standard |
ASTM A283, ASTM A573, ASTM A283M, ASTM A29M, ASTM A529M, ASTM A572M, ASTM A588M, ASTM A663M, ASTM A678M, ASTM A808, DIN EN10025, JIS G3101, JIS G3101, JIS G3101, JIS G3131, JIS G3131, JIS, 1, JIS G3506 , GB/T700, GB/T699, GB/T1591, GB/T3077 |
|
|
Materjal |
Q235, Q345, Q420, 20#, 35#, 45#, 16 min |
|
|
Pind |
Poleerimine, lõõmutamine, marineerimine, hele |
|
|
Tüüp |
kuumvaltsitud |
|
|
Ümmargune toru/toru |
||
|
Suurus |
seina paksus |
1mm-150mm |
|
Väline diameeter |
6mm-2500mm (3/8"-100") |
|
ASTM A333 keemilise koostise nõuded
| ASTM A333 keemiline koostis | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Element | Hinne 1, % | Hinne 3, % | Hinne 4, % | Hinne 6, % | Hinne 7, % | Hinne 8, % | Hinne 9, % | Hinne 10, % | Hinne 11, % |
| C | 0.30 | 0.19 | 0.12 | 0.30 | 0.19 | 0.13 | 0.20 | 0.20 | 0.10 |
| Mn | 0.40–1.06 | 0.31–0.64 | 0.50–1.05 | 0.29–1.06 | 0.90 | 0.90 | 0.40–1.06 | 1.15–1.50 | 0.60 |
| P | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.035 | 0.025 |
| S | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.015 | 0.025 |
| Si | ... | 0.18–0.37 | 0.08–0.37 | 0.10 min | 0.13–0.32 | 0.13–0.32 | ... | 0.10–0.35 | 0.35 |
| Ni | ... | 3.18–3.82 | 0.47–0.98 | 0.40 | 2.03–2.57 | 8.40–9.60 | 1.60–2.24 | 0.25 | 35.0–37.0 |
| Kr | ... | ... | 0.44–1.01 | 0.30 | ... | ... | ... | 0.15 | 0.50 |
| Cu | ... | ... | 0.40–0.75 | 0.40 | ... | ... | 0.75–1.25 | 0.15 | ... |
| Al | ... | ... | 0.04–0.30 | ... | ... | ... | ... | 0.06 | ... |
| V | ... | ... | ... | 0.08 | ... | ... | ... | 0.12 | ... |
| Cb | ... | ... | ... | 0.02 | ... | ... | ... | 0.05 | ... |
| Mo | ... | ... | ... | 0.12 | ... | ... | ... | 0.05 | 0.50 |
| Kaas | ... | ... | ... | ... | ... | ... | ... | ... | 0.50 |